Diamond Blade Selection Chart

Match three things and you cannot go far wrong: the rim type to the material, the diameter to the machine, and the RPM rating to the spindle speed. The tables below cover all twelve TUSKO series with the diameter range and arbor each one is made in.

1. Choose the series by material

Material / applicationSeriesDiameterArbor
Concrete, paving slabs, brickworkTS segmented115-350 mm22.2 / 25.4 mm
Reinforced concrete, hard aggregateTSO ordered (laser welded)115-350 mm22.2 / 25.4 mm
Granite, engineered stone, cured concreteTT turbo115-230 mm22.2 mm
Porcelain, ceramic tile, chip-free cutsTN continuous105-230 mm20 / 22.2 mm
Marble, travertine, natural stoneTC continuous for stone110-230 mm20 / 22.2 mm
Roads, asphalt, wall sawingTR large diameter350-800 mm25.4 / 60 mm
Kerb stones, roofing tiles, green concreteTSB brazing115-230 mm22.2 mm
Angle grinder, fast dry cuttingTSF mesh turbo115-125 mm22.2 mm
Floor coating removal, concrete grindingTG grinding plate100-180 mm22.2 mm
Core drilling, reinforced concreteCD core drill8-1000 mmthreaded / hex
Deep holes, replaceable cutter headThreaded tube26-300 mmthreaded
Granite, marble, tile drillingStone hole saw6-165 mmtriangular shank

Diameter and arbor figures are the standard production range of each series; other sizes are made to order.

2. Maximum spindle speed by blade diameter

Rim speed is what actually limits a blade, not diameter on its own. The table converts a 60 m/s working rim speed and an 80 m/s maximum into spindle RPM for each common diameter, so you can check a blade against any machine.

Blade diameterRPM at 60 m/sRPM at 80 m/sTypical machine
100 mm11,45915,279Angle grinder
115 mm9,96413,286Angle grinder
125 mm9,16712,223Angle grinder
150 mm7,63910,186Large angle grinder
180 mm6,3668,488Large angle grinder
230 mm4,9826,643Large angle grinder
300 mm3,8205,093Cut-off saw
350 mm3,2744,365Cut-off saw
400 mm2,8653,820Floor saw
450 mm2,5463,395Floor saw
500 mm2,2923,056Floor saw
600 mm1,9102,546Wall saw
800 mm1,4321,910Wall saw

Calculated with RPM = rim speed × 60,000 ÷ (π × diameter). Always use the lower of the two numbers when the blade label states a maximum RPM.

3. What the rim type actually does

Segmented

Deep gullets clear slurry and debris, so the blade stays cool and cuts fast. Best in concrete, brick and asphalt where finish does not matter.

Turbo

A serrated continuous edge: faster than a continuous rim, cleaner than a segmented one. The general-purpose choice for granite and hard concrete.

Continuous

No gullets, so the edge stays intact and the cut is chip-free. The only correct choice for porcelain and polished stone, and it needs water.

Frequently asked questions

How do I choose a diamond blade for concrete?

Use a segmented rim for cured concrete, paving slabs and general building work where fast cutting matters more than a clean edge. For reinforced concrete, switch to a laser-welded ordered rim, which holds the diamond in the matrix when it meets rebar. Continuous rims are the wrong choice here: they cut slowly and overheat.

What does the maximum RPM on a blade mean?

It is the highest spindle speed the blade is rated for, set by the rim speed the bond can survive. A 115 mm blade rated for 13,000 rpm is safe on a standard 11,000 rpm angle grinder; a 350 mm blade rated for 4,300 rpm must never go on a machine running faster. Always check the blade label against the machine's no-load speed.

Which arbor size do I need?

22.2 mm is the standard bore for 100-230 mm angle grinder blades worldwide. Large blades use 25.4 mm or a 60 mm drive hole for floor saws and wall saws, while core drills use a threaded or hex drive depending on the rig. If your machine uses a different spindle, a reducing ring solves it.

What is the difference between segmented, turbo and continuous rims?

Segmented rims have deep gullets that clear debris fast, so they cut quickly in abrasive material. Turbo rims have a serrated continuous edge that cuts fast but leaves a cleaner finish. Continuous rims have no gullets at all, which gives a chip-free edge in tile, porcelain and marble but limits speed and requires water.

Why does my diamond blade stop cutting?

Almost always glazing: the diamond segments polish over because the blade is cutting soft abrasive material at too low a pressure, or running without enough water. Cut a few passes through an abrasive block or hard concrete to expose fresh diamond, then reduce spindle speed and check water flow.